Equistar Petrothene® NA340212 Low Density Polyethylene, Film Extrusion Grade

 

Subcategory: Polyethylene; LDPE; Equistar Low Density Polyethylene; Equistar Polyethylene

Material Notes:
PETROTHENE NA340 is a series of LDPE/EVA copolymer resins designed for quality bags and special film applications that require clarity and excellent impact strength. Typical applications include heavy produce, textile and frozen food packaging. No Slip, High Antiblock.

Regulatory Status: NA340 resins meet the requirements of the Food and Drug Administration regulation 21 CFR 177.1350. This regulation allows the use of this ethylene vinyl acetate copolymer "...in articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for further information.

NA340 resins are processed readily by standard blown film extrusion techniques. A processing melt temperature of 330°-375°F (165°-191°C) is suggested for this resin. Specific recommendations for the processing of NA 340 can only be made when the processing conditions, equipment and end use are known. For further suggestions, contact your Equistar sales representative.

Available Properties
  • Vinyl Acetate Content
  • Thickness
  • Melt Flow
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Elmendorf Tear Strength MD
  • Elmendorf Tear Strength TD
  • Dart Drop
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • 1% Secant Modulus, MD
  • 1% Secant Modulus, TD
  • Vicat Softening Point
  • Slip
  • Haze
  • Gloss
  • Melt Temperature
  • Die Opening
  • Blow-up Ratio (BUR)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。