Equistar Alathon® H5220 High Density Polyethylene, Injection Molding Grade
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer; Equistar High Density Polyethylene; Equistar Polyethylene
Key Words: FDA 21 CFR 177.1520.
Material Notes: Applications Alathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications include housewares, containers, caps and closures.Regulatory Status H5220 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. Processing Techniques Specific recommendations for processing H5220 can only be made when the processing conditions, equipment and end-use applications are known.
| Available Properties |
- Density
- Bulk Density
- Melt Flow
- Spiral Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- 1% Secant Modulus
- Izod Impact, Notched
- Izod Impact, Notched @ -18°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|