Equistar Microthene® MP564189 Linear Low Density Polyethylene, Injection Molding Grade
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer; Equistar Linear Low Density Polyethylene; Equistar Polyethylene
Key Words: FDA 21 CFR 177.1520.
Material Notes: Applications Microthene MP564189 exhibits good stiffness and low temperature toughness. Typical applications include trash cans, industrial containers, housewares and toys. MP564189 is 16 mesh powder and is also available in pellet form Petrothene GA564189.Regulatory Status MP564189 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. Processing Techniques Specific recommendations for processing MP564189 can only be made when the processing conditions, equipment and end use are known.
| Available Properties |
- Density
- Melt Flow
- Spiral Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- 1% Secant Modulus
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|