Equistar Petrothene® NA247000 Low Density Polyethylene, Injection Molding Grade
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer; Equistar Low Density Polyethylene; Equistar Polyethylene
Key Words: FDA 21 CFR 177.1520.
Material Notes: Applications Petrothene NA247000 provides a balance of stiffness and tear strength. Typical applications include tamper evident caps and closures.Regulatory Status NA247000 meets the requirements of the Food and Drug Administration, regulation 21 CFR 177.1520. Processing Techniques Specific recommendations for processing NA247000 can only be made when the processing conditions, equipment and end use are known.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Brittleness Temperature
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|