Equistar Petrothene® NA373242 Low Density Polyethylene, Cast/Blown Film Grade
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer; Equistar Low Density Polyethylene; Equistar Polyethylene
Key Words: FDA 21 CFR 177.1520.
Material Notes: Applications Petrothene NA373 is a series of homopolymer resins selected by customers for use in household film and other applications that require high clarity and good impact strength combined with low COF.Regulatory Status The basic NA373 resin meets the requirements of the Food and Drug Administration, regulation 21 CFR 177.1520. Processing Techniques Specific recommendations for processing NA373 resins can only be made when the processing conditions, equipment and end use are known.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Antiblock Level
- Slip Level
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Dart Drop Test
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Haze
- Gloss
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|