Eurotec® Tecodur® PB70 GR30 NL XA 20 PBT 30% glass fiber reinforced, UL94 V0
Subcategory: Polybutylene Terephthalate (PBT); Thermoplastic; Polymer
Material Notes:
- Excellent stiffness and hardness
- Good mechanical strength
- Good creep and fatigue behavior
- Very good thermal stability
- Excellent flammability characteristics
- Good electrical properties
- High wear resistance and low friction
- Good dimensional stability
- Very good chemical resistance
- Excellent flow and processing properties
- Low moisture absorption
- Very good surface finish
APPLICATIONS: - Automotive
- Electrical/Electronic
- Business equipment
- Construction
- Home appliances
| Available Properties |
- Density
- Filler Content
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Izod Impact, Notched (ISO)
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Comparative Tracking Index
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Glow Wire Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|