EVAL® EP-J102B Ethylene Vinyl Alcohol Copolymer Resin
Subcategory: Ethylene Vinyl Alcohol; Thermoplastic; Polymer
Key Words: EVOH; EVALCA; EVAL Company of America; Ethylene Vinylalcohol
Material Notes: 32 mol % Ethylene.Data provided by EVALCA. Designed to provide a wide thermoforming range together with high barrier properties. EVAL® EP-J102B is specifically designed for thermoforming applications using polystyrene and polyethylene structural layers. This resin can be used with SPPF or melt phase forming techniques. EVOH is used in packaging applications because of its outstanding gas barrier properties.
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Melt Flow
- Hardness, Rockwell M
- Film Tensile Strength at Break, MD
- Film Elongation at Break, MD
- Tensile Strength, Yield
- Modulus of Elasticity
- Dielectric Constant
- Dissipation Factor
- CTE, linear 20°C
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Glass Temperature
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|