EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin
Subcategory: Ethylene Vinyl Alcohol; Thermoplastic; Polymer
Key Words: EVOH; EVALCA; EVAL Company of America; Ethylene Vinylalcohol
Material Notes: 44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas barrier properties.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Moisture Vapor Transmission
- Oxygen Transmission
- Melt Flow
- Hardness, Rockwell M
- Film Tensile Strength at Break, MD
- Film Elongation at Break, MD
- Tensile Strength, Yield
- Modulus of Elasticity
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
- CTE, linear 20°C
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Glass Temperature
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|