EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film
Subcategory: Ethylene Vinyl Alcohol; Thermoplastic; Polymer
Key Words: EVOH; EVALCA; EVAL Company of America; Ethylene Vinylalcohol
Material Notes: 44 mol % Ethylene. Non oriented type film; property values for 20 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier properties.
| Available Properties |
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Moisture Vapor Transmission
- Oxygen Transmission
- Thickness
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dissipation Factor
- CTE, linear 20°C
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|