ExxonMobil EVA LD 312.82 High Impact Film Resin
Subcategory: Ethylene Vinyl Acetate; Thermoplastic; Polymer
Material Notes: LD 312 Series films have superior impact strength, good heat sealability, and good low temperature properties. Applications include frozen and other food packaging. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Vinyl Acetate Content
- Thickness
- Melt Flow
- Antiblock Level
- Slip Level
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Film Elongation at Yield, MD
- Film Elongation at Yield, TD
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Dart Drop Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Melting Point
- Crystallization Temperature
- Vicat Softening Point
- Haze
- Gloss
- Features
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|