ExxonMobil LDPE LD 206.48 Extrusion Coating Resin
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: LD 206.48 is a extrusion coating grade, having good organoleptic properties compared to existing standard low odor/off-taste LDPE extrusion coating polymers. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Melt Flow
- Neck In
- Drawdown
- Melting Point
- Vicat Softening Point
|
|
|
|