ExxonMobil LDPE LD 509.48 Compounding Resin
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: LD 509.48 is a high melt index homopolymer resin designed to provide good processability in compounding applications. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Film Elongation at Break, MD
- Tensile Strength @ Yield
- 1% Secant Modulus
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|