ExxonMobil HDPE HD 6605.70 Injection Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: HD 6605 is a narrow molecular weight hexene copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balance. Ideally suited for articles requiring rugged physical performance in cold temperature environments. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Tensile Impact Strength
- Izod Impact, Notched
- Melting Point
- Crystallization Temperature
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Brittleness Temperature
- Features
- Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|