ExxonMobil HDPE HD 7845.30 MMW Blown Film Resin
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer
Material Notes: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides excellent film appearance and high quality recycle. HD 7845.30 is particularly recommended as a blend component with LLDPE for stiff clear films. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Features
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|