ExxonMobil HDPE HD 9856BA Blow Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: HD 9856BA is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856BA exhibit a unique combination of stiffness and environmental stress cracking resistance. These properties, coupled with excellent processability on both continuous and intermittent equipment, afford significant lightweighting and/or fast cycling potential in many applications. HD 9865BA contains an antistat which may be used in contact with limited types of food. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Bulk Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Tensile Impact Strength
- Brittleness Temperature
- Features
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|