ExxonMobil Paxon™ HDPE 7003 Crosslinkable Rotational Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: 7003 is a UV-stabilized, crosslinkable HDPE, supplied as pellets, intended for use in rotational molding. Properly molded parts made with 7003 show exceptional environmental stress cracking resistance. The high flow base resin promotes rapid melting and outstanding part fill during processing while the finished part exhibits high performance characteristics reflecting crosslinked molecular weight. This resin is available in various colors, plus natural. Crosslink Potential measured to be 2.5 by ExxonMobil method. Information provided by ExxonMobil Chemical
| Available Properties |
- Bulk Density
- ESCR 10% Igepal®
- Tensile Strength @ Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
- Features
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|