ExxonMobil Paxon™ HDPE BA7718 Sheet Extrusion and Blow Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: BA7718 is a 25% brown mica-filled, medium molecular weight, high density polyethylene. This material has been specifically developed as a cost effective resin for applications which require outstanding stiffness and heat deflection temperatures. This material is designed for increased rigidity, dimensional stability, warpage resistance, and heat deflection temperatures compared to conventional HDPE. Resin must be dried just prior to the blow molding or sheet extrusion process. Information provided by ExxonMobil Chemical
| Available Properties |
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Gardner Impact @ 23°C
- Tensile Impact Strength
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|