ExxonMobil Exceed™ mLLDPE 2018CA Blown Film Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: Exceed 2018CA resin is an ethylene based polymer produced with metallocene single site catalysts using ExxonMobil Chemicals EXXPOL® Technology. The higher melt index makes this polymer ideally suited for blending into LDPE rich films as well as skin layer in coextrusion applications. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tear Strength
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Melting Point
- Haze
- Gloss
- Features
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|