ExxonMobil ESCORENE™ ULTRA EVA LD 755.12 Molding, extrusion and compounding resin
Subcategory: Ethylene Vinyl Acetate; Thermoplastic
Material Notes: Escorene Ultra LD 755.12 is a high vinyl acetate copolymer for specialty compounding applications and hot melt adhesives. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Vinyl Acetate Content
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Impact Test
- Melting Point
- Features
|
|
|
|