ExxonMobil ESCORENE™ ULTRA UL 7510 Adhesive Application Resin
Subcategory: Adhesive; Ethylene Vinyl Acetate; Thermoplastic
Material Notes: Escorene Ultra UL 7510 is a very high flow, 19.5% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, sealants and wax blends. Information provided by ExxonMobil Chemical