ExxonMobil ESCORENE™ ULTRA UL 8705 Adhesive Application Resin
Subcategory: Adhesive; Ethylene Vinyl Acetate; Thermoplastic
Material Notes: Escorene Ultra UL 8705 is a relatively low viscosity, 29% vinyl acetate copolymer specifically tailored for enhanced modulus/tensile performance at the same viscosity of similar materials. It has good compatibility with both hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt adhesives, glue sticks, sealants and wax blends. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Viscosity
- Vinyl Acetate Content
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Melting Point
- Features
|
|
|
|