ExxonMobil OPTEMA™ EMA TC 115 Molding, extrusion and compounding resin
Subcategory: Ethylene Methyl Acrylate; Thermoplastic
Material Notes: OPTEMA TC 115 is an ethylene methyl acrylate copolymer, which can be used as a compatibilizer and impact modifier for engineering thermoplastics. It has been processed at temperatures up to 625°F without thermal degradation. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Methyl Acrylate Content
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Impact Test
- Melting Point
- Vicat Softening Point
- Features
|
|
|
|
| Property Data |