ExxonMobil OPTEMA™ EMA TC 120 Molding, extrusion and compounding resin
Subcategory: Ethylene Methyl Acrylate; Thermoplastic
Material Notes: OPTEMA TC 120 is an ethylene methyl acrylate copolymer, which can be used as an impact modifier or compatibilizer in polymer compounds. It has been processed on typical LDPE compounding equipment at temperatures up to 625°F. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Methyl Acrylate Content
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Impact Test
- Melting Point
- Vicat Softening Point
- Features
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|