ExxonMobil OPTEMA™ EMA TC 130 Molding, extrusion and compounding resin
Subcategory: Ethylene Methyl Acrylate; Thermoplastic
Material Notes: OPTEMA TC 130 is an ethylene methyl acrylate copolymer, which can be used in specialty applications such as a carrier for color and additive master batches, a compatibilizer in polymer compounds and hot melt adhesives. It can been processed at temperatures as low as 200°F and up to 600°F. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Methyl Acrylate Content
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Impact Test
- Melting Point
- Vicat Softening Point
- Features
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|