ExxonMobil ESCOR™ EMA-AA AT 310 Blown Film Resin
Subcategory: Ethylene Acrylic Acid; Ethylene Methyl Acrylate; Thermoplastic; Polymer
Material Notes: ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable for use as a polymer modifier to improve adhesion. Information provided by ExxonMobil Chemical
| Available Properties |
- Methyl Acrylate Content
- Acrylic Acid Content
- Melt Flow
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Melting Point
- Features
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|