ExxonMobil ESCOR™ EMA-AA AT 320 Cast Film Resin
Subcategory: Ethylene Acrylic Acid; Ethylene Methyl Acrylate; Thermoplastic; Polymer
Material Notes: ESCOR AT 320 provides excellent adhesion to a variety of substrates and other film components such as aluminum foil, polyolefins, polycarbonate, PET, etc. Information provided by ExxonMobil Chemical
| Available Properties |
- Methyl Acrylate Content
- Acrylic Acid Content
- Melt Flow
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Melting Point
- Haze
- Gloss
- Features
|
|
|
|
| Property Data |