ExxonMobil POLYBILT™ PB 103E Bitumen Modifier Resin
Subcategory: Ethylene Vinyl Acetate; Thermoplastic
Material Notes: Polybilt PB 103E is an 33% VA copolymer that yields modified bitumen blends with good storage stability, increased softening point, increased high temperature viscosity and decreased penetration. PB 103E can be blended using conventional equipment, Blending time will depend on the shear rate of the equipment used and temperature. The recommended temperature range is 330 to 350°F. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Vinyl Acetate Content
- Melt Flow
- Melting Point
- Features
|
|
|
|
| Property Data |