ExxonMobil LLDPE LL 6202 Injection Molding Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE
Material Notes: LL 6202 is a narrow molecular weight butene copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that require outstanding tear resistance and low warpage. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Tensile Impact Strength
- Melting Point
- Crystallization Temperature
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|