ExxonMobil LLDPE LL 3201.22 Premium High Strength Film Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: LL 3201 resins are hexene copolymer LLDPE film resins. Films produced from these resins have excellent tensile, toughness and stiffness properties. These strength properties, along with good drawdown capability, permit usage in many demanding packaging applications. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Thickness
- Melt Flow
- Antiblock Level
- Slip Level
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Impact Test
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Melting Point
- Haze
- Gloss
- Features
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|