ExxonMobil LLDPE LL 8450 Rotational Molding Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE
Material Notes: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. This resin is ideally suited for applications that require optimum balance stiffness and processability. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- ESCR 100% Igepal®
- ESCR 10% Igepal®
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Impact Test
- Melting Point
- Crystallization Temperature
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|