ExxonMobil NTX™ LLDPE NTX 095 Super Strength Film Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impact and tear strength. NTX resins are formulated with various additive packages for use in all high performance film applications. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Thickness
- Melt Flow
- Antiblock Level
- Slip Level
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Features
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|