ExxonMobil EXXCO™ Polyethylene Exxco 012 w/20% LDPE Enhanced Performance Extrusion Coating Resin
Subcategory: Polyethylene; Thermoplastic
Material Notes: Exxco 012 PE resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. It offers outstanding adhesion to many substrates, along with excellent hot tack and heat seal strengths. It can be used as a minority or majority component with LDPE to improve toughness and heat sealing performance. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Melt Flow
- Neck In
- Drawdown
- Melting Point
- Vicat Softening Point
- Features
|
|
|
|
| Property Data |