ExxonMobil PP PP1024E4 Homopolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Medium melt flow rate homopolymer. Particularly suitable for general purpose injection molding applications. Information provided by ExxonMobil Chemical