ExxonMobil PP PP1043F Mineral-filled Homopolymer
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Medium melt flow rate homopolymer, 40% filled. Particularly suitable for injection molding applications requiring long term heat aging resistance. UL continuous service rating of 90°C Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
|
|
|
|