ExxonMobil PP PP3546G Homopolylmer Grade for Ultra-High Melt Flow Rate Nonwoven Applications
Subcategory: Polypropylene; Thermoplastic
Material Notes: Free-flowing, low-dusting granular resin for melt blown nonwoven applications. Peroxide added to control the polymer rheology during processing Information provided by ExxonMobil Chemical
| Available Properties |
- Particle Mesh Size
- Melt Flow
- Processing Temperature
|
|
|
|
| Property Data |