ExxonMobil PP PP8114E1 Impact Copolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Super high impact copolymer with excellent processing attributes. Particularly suitable for automotive interior applications requiring ductility at low temperature.Automotive Certifications: GM: GMP.PP.107Ford: WSS-M4D638-CDaimler-Chrysler: MS DB588 and MS DB500 CPN 4017 Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Gardner Impact @ -30°C
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Processing Temperature
|
|
|
|