ExxonMobil PP PP8224E1 Impact Copolymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: Super high impact copolymer with excellent processing attributes. Particularly suitable for automotive exterior applications requiring ductility at low temperature.Automotive Certifications: Ford: WSS-M4D952-A1Daimler-Chrysler: MS DC256 Type A CPN 4131, 3403, 3506, 4161 Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Yield
- Flexural Modulus
- Impact Test
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Processing Temperature
|
|
|
|
| Property Data |