Exxon™ SB Bromobutyl 6222 Brominated Star-Branched Butyl
Subcategory: Elastomer, TS; Thermoset
Material Notes: Exxon SB Bromobutyl is a brominated copolymer of isobutylene and isoprene, including a styrene block copolymer branching agent. Information provided by ExxonMobil Chemical
| Available Properties |
- Specific Gravity
- Mooney Viscosity
- Cure Time
- Anti oxidant
- Bromine
- cure MH
- cure ML
- Water
|
|
|
|