ExxonMobil Vistalon™ 1703P EPDM
Subcategory: Elastomer, TS; Thermoset
Material Notes: An EPDM for wire and cable insulation Information provided by ExxonMobil Chemical
| Available Properties |
- Mooney Viscosity
- Ethylene Content, %
- VNB Content, %
|
|
|
|
| Property Data |