ExxonMobil EXACT™ 4151 Plastomer for Cast Film
Subcategory: Elastomer, TPE; Thermoplastic; Polymer
Material Notes: Ethylene based hexene plastomer produced using ExxonMobil Chemical Exxpol technology. Designed for use in both monolayer and multilayer coextruded cast and blown film applications requiring low sealing temperatures, high oxygen transmission and high toughness. Typical applications include seal layers for lamination films used in meat, poultry and produce packaging. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Film Elongation at Yield, MD
- Film Elongation at Yield, TD
- Impact Test
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Melting Point
- Crystallization Temperature
- Vicat Softening Point
- Haze
- Gloss
- Features
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|