ExxonMobil EXACT™ 8203 Octene-1 Plastomer
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: Ethylene based octene plastomer produced in a solution polymerization process using a metallocene catalyst. Designed for applications requiring high flexibility, outstanding toughness, excellent low temperature flex-cracking resistance and high clarity. This material combines favorable melt strength with an excellent processability, offering important advantages for foam, wire and cable and extrusion applications. Suitable for improving the impact resistance or flexibility of molded polyolefins. Information provided by ExxonMobil Chemical
| Available Properties |
- Density
- Mooney Viscosity
- Environmental Stress Crack Resistance
- Thickness
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Impact
- Dart Drop
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Izod Impact, Notched @ -40°C
- Izod Impact, Notched
- Heat Seal Strength Initiation Temperarture
- Heat of Fusion
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|