ExxonMobil Bicor® 110 AXT OPP Film
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Two sided coated, sealable OPP film designed for delivering an advanced level of moisture and oxygen barrier protection. This film is designed for use in horizontal or vertical packaging. This film is also used as an outer web of laminations for gas-flush applications. Information provided by ExxonMobil Chemical
| Available Properties |
- Water Vapor Transmission
- Oxygen Transmission Rate
- Thickness
- Coating Weight
- Coefficient of Friction
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Shrinkage, MD
- Shrinkage, TD
- Haze
- Gloss
- Crimp Seal MST, °F
- Crimp Seal Strength, g/in
- Yield, in2/lb
|
|
|
|
| Property Data |