ExxonMobil Bicor® 30 GBL OPP Film
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: One-side PVdC-coated OPP film designed for use in pet food packaging. The PVdC coating provides grease resistance, a modified core for puncture resistance, and a modified sealant layer for improved seals and hot melt adhesion. Information provided by ExxonMobil Chemical
| Available Properties |
- Water Vapor Transmission
- Oxygen Transmission Rate
- Thickness
- Coating Weight
- Coefficient of Friction
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Shrinkage, MD
- Shrinkage, TD
- Haze
- Crimp Seal MST, °F
- Crimp Seal Strength, g/in
- Yield, in2/lb
|
|
|
|