ExxonMobil Bicor® 120 SPW OPP Film
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: One-side treated, one-side sealable, coextruded OPP film designed for use in plain, unsupported applications and in lamination to itself. It may be used in HFFS and VFFS applications. The treated high energy layer provides an excellent surface for converter processing. Information provided by ExxonMobil Chemical
| Available Properties |
- Water Vapor Transmission
- Thickness
- Coating Weight
- Coefficient of Friction
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Shrinkage, MD
- Shrinkage, TD
- Haze
- Gloss
- Crimp Seal MST, °F
- Crimp Seal Strength, g/in
- Wetting Tension, receding COS theta
- Yield, in2/lb
|
|
|
|