ExxonMobil OPPalyte® 295 HSTW OPP Film
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: One-side coated, white opaque OPP film with a proprietary cavitated core. It is designed for use unsupported or in a lamination for heat seal or cold seal packaging applications. One side is treated. Information provided by ExxonMobil Chemical
| Available Properties |
- Water Vapor Transmission
- Oxygen Transmission Rate
- Thickness
- Coating Weight
- Coefficient of Friction
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Shrinkage, MD
- Shrinkage, TD
- Gloss
- Transmission, Visible
- Wetting Tension, receding COS theta
- Yield, in2/lb
|
|
|
|
| Property Data |