ExxonMobil OPPalyte® 245 STW OPP Film
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: One-side sealable OPP film with a translucent white appearance. STW was designed on ice cream novelty, multi-lane equipment. It is also well suited for HFFS and VFFS machines. Can be used as a monoweb structure or as the inside web of a lamination. Information provided by ExxonMobil Chemical
| Available Properties |
- Water Vapor Transmission
- Thickness
- Coating Weight
- Coefficient of Friction
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Shrinkage, MD
- Shrinkage, TD
- Gloss
- Transmission, Visible
- Crimp Seal MST, °F
- Crimp Seal Strength
- Yield, in2/lb
|
|
|
|