ExxonMobil Metallyte® 70 MET-HB OPP Film
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Vacuum-metallized, high barrier OPP film with a proprietary sealant layer. This film offers excellent moisture and oxygen barriers, hot tack, seal integrity, and lap seal range when used with a coextruded outer web. MET-HB is designed specifically for adhesive and craze-free extrusion laminations. Information provided by ExxonMobil Chemical
| Available Properties |
- Water Vapor Transmission
- Oxygen Transmission Rate
- Thickness
- Coating Weight
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Shrinkage, MD
- Shrinkage, TD
- Optical Density
- Transmission, Visible
- Crimp Seal MST, °F
- Crimp Seal Strength
- Yield, in2/lb
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|