ExxonMobil Metallyte® 28 MWHB OPP Film
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Multi-layer, cavitated, white OPP film that has exceptional barrier to gases, flavors and moisture. It is metallized on one side with a proprietary sealant layer on the other. MWHB is lap sealable to other coextruded OPP films. It is designed specifically for adhesive and craze-free extrusion laminations aw well as converted monoweb applications. Information provided by ExxonMobil Chemical