ExxonMobil Hicor® 30 HT 103 OHD Film
Subcategory: Thermoplastic; HDPE; Polymer
Material Notes: One-side treated, non-sealable, oriented high density polyethylene film, which has outstanding stiffness, deadfold, and directional tear characteristics. This film has been designed to be used in various applications, such as twistwrap and laminated to other ExxonMobil Chemical OPP films, providing a new generation of laminates. Information provided by ExxonMobil Chemical
| Available Properties |
- Water Vapor Transmission
- Thickness
- Coating Weight
- Coefficient of Friction
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Shrinkage, MD
- Shrinkage, TD
- Haze
- Gloss
- Yield, in2/lb
|
|
|
|