ExxonMobil Hicor® 30 HT 183 OHD Film
Subcategory: Thermoplastic; HDPE; Polymer
Material Notes: One-side metallized, non-sealable, oriented high density polyethylene film, which has outstanding deadfold and directional tear characteristics. This film has been designed to be used in various applications, such as twistwrap and in laminations with other ExxonMobil Chemical OPP films, providing a new generation of laminates. Information provided by ExxonMobil Chemical